EVA foam (closed cell)

2019-12-23 04:54:52

projectunitperformance indexApparent densityg cm30 08-0 12tensile strengthKpa≥1000tear strengthN cm≥4 5elongation at b



 

project unit performance index
Apparent density g/cm3 0.08-0.12
tensile strength Kpa ≥1000
tear strength N/cm ≥4.5
elongation at break % ≥100
Low temperature resistance - The sample is kept at - 50 ℃ for 0.5 hours without obvious change
 
High temperature resistance - The sample was kept at 70 ℃ for 24 hours without obvious change
 
compressive strength(25%) % ≥100
Features and uses:
 
1. Excellent elasticity and compression properties.
 
2. Widely used in automobile, air conditioning industry.